A new nitrogen added alloy from Lohmanns Stahl, Germany. Designed for knife applications that require improved corrosion resistance and edge holding such as knives for fish, or knives used in a saltwater environment.
Chemical Composition:-
C:
|
Cr:
|
Mo:
|
V:
|
N:
|
0.6%
|
17%
|
1.1%
|
0.1%
|
0.25%
|
Suggested Heat Treatments:
Heat to 1000 - 1040C (Hold for 10 minutes)
Oil Quench (Suggested Oil is Rye 32)
Temper twice for two hours at 260C for approx 56HRc
Supplied Hot Rolled Annealed in 600mm Lengths